Prediction of maximum pitting corrosion depth in oil and gas pipelines

Mohamed El Amine Ben Seghier, Behrooz Keshtegar, Kong Fah Tee, Tarek Zayed, Rouzbeh Abbassi, Nguyen Thoi Trung

Research output: Journal article publicationJournal articleAcademic researchpeer-review

57 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Prediction of maximum pitting corrosion depth in oil and gas pipelines'. Together they form a unique fingerprint.