(Na0.475K0.475Li0.05)(Nb0.92Ta0.05Sb0.03)O3lead-free ceramics with addition of CeO2

T. Lee, Kin Wing Kwok, H. L.W. Chan

Research output: Chapter in book / Conference proceedingConference article published in proceeding or bookAcademic researchpeer-review

Abstract

Lead-free piezoelectric ceramics (Na0.475K0.475Li0.05)(Nb0.92Ta0.05Sb0.03)O3added with different amounts of CeO2have been prepared by a conventional mixed-oxide method. After the addition of CeO2, the sintering performance of the ceramics is greatly improved. The ceramics can be well-sintered at a higher temperature, and hence have a higher density and better piezoelectric and dielectric properties. For the ceramic added with 0.4 wt% CeO2, the piezoelectric and dielectric properties become optimum, giving d33= 246 pC/N, kp= 0.50, εr= 1300 and tanδ= 4%.
Original languageEnglish
Title of host publication2007 16th IEEE International Symposium on the Applications of Ferroelectrics, ISAF
Pages667-669
Number of pages3
DOIs
Publication statusPublished - 1 Dec 2007
Event2007 16th IEEE International Symposium on the Applications of Ferroelectrics, ISAF - Nara-city, Japan
Duration: 27 May 200731 May 2007

Conference

Conference2007 16th IEEE International Symposium on the Applications of Ferroelectrics, ISAF
Country/TerritoryJapan
CityNara-city
Period27/05/0731/05/07

ASJC Scopus subject areas

  • Electronic, Optical and Magnetic Materials
  • Electrical and Electronic Engineering

Fingerprint

Dive into the research topics of '(Na0.475K0.475Li0.05)(Nb0.92Ta0.05Sb0.03)O3lead-free ceramics with addition of CeO2'. Together they form a unique fingerprint.

Cite this